Customized HSS Roll

Availability:
Quantity:
HBW has a complete production infrastructure, with a qualified technical team and high-performance products, guaranteeing customers the most modern and efficient products for their applications.
If you’re looking for custom-made mill rolls for various applications, then make sure to check out our products. We provide a range of customized mill rolls for all your different operations. Moreover, we use durable Alloy materials such as Tungsten、Manganese、Vanadium、Molybdenum etc. to meet all your demands


◆◇ Unique Features

  • High V, W, Cr, Mo, Nb and other alloy elements. Carbide types: MC and M2C  with high hardness and good abrasion resistance.

  • Excellet thermal stability, high hardness and good wear resistance. 

  • High expansion coefficient and good thermal conductivity, more conducive to control.

  • Forming oxide film during rolling process, improving roll wear resistance significantly.

  • Super high strength of the roll core (DCI).


◆◇ Specification

Specification

280-850mm roll body diameter

Hardness

73-98 HSD

Surface Roughness

Ra0.05

Standard

GB/T1503-2008

Machining Tolerance

+/-0.01mm

Quality Certification

ISO9001:2015

Single Weight

Max 10 Tons/PC

Multiple Thread Holes

Acceptable

Deep Holes

Acceptable

Customized Roughness

Acceptable

Inspection

100% Inspection

Transport Package

Anti-rust and Waterproof packing  layed in a Metallic Framework

Taper

Acceptable

The End of The Roll Is Slotted

Acceptable

Slotted of Roll

Acceptable

Deep Thread Holes

Acceptable

Coating

Anticorrosive Paint

Application

Finishing Rolls for Hot Strip Steel, Wire and Rod


Universal Mills for Section Steel


Finishing Rolls for Hot Strip Steel, Wire and Rod


◆◇ Chemical Analysis

Material

HBW Patented Chemical Composition (%)

C

Si

Mn

Cr

Ni

Mo

V

W

P & S

Nb

Co

Others

HSS

(Alloy composition changes based on different grades)

1.5

~

2.10

0.3

~

1.0

0.30

~

0.70

3.00

~

6.00

0.50

~

1.50

3.0

~

7.0

2.0

~

8.0

1.0

~

8.0

≤0.03

Depends on HSS Grade


◆◇ Physical Properties

Properties Barrel Core
Tensile Strength ≥700MPa ≥450MPa
Compressive Strength ≥2500MPa --


◆◇ We Offer the Following Services:

  • Technical Drawings

  • Alloy Chemical Composion Range

  • Surface and Size Inspection Report

  • Customized Lettering on surface of products


We deliver end -to -end solutions and help in setting up,running and optimising mill rolling through our products and engineering services. and help in solving the challenges faced by the rolling mill industry today.

Previous: 
Next: 

CONTACT US

Phone: +86-13866508328
Tel: +86-562-2610227
Email:  export@hbwroll.com
WhatsApp: +8613866508328
Add: No. 699 Wusongshan Avenue, Tongling City, Anhui Province, China 244000

QUICK LINKS

PRODUCTS

SIGN UP FOR OUR NEWSLETTER

Copyright © 2026 Anhui Huanbowan High Speed Steel Mill Roll Co.,Ltd. All Rights Reserved.  Sitemap.  Privacy Policy.   皖ICP备15013066号-4